Titanium diboride (TiB2) is a novel sintered ceramic material which has attracted a great deal of interest because of its excellent mechanical properties, wear resistance and chemical resistance. At present, this ceramic is used in specialized applications in such areas as impact resistant armor, cutting tools, crucibles and wear resistant coatings. In this present research work, effects of current intensity, pulse time and duty cycle on the spacing roughness parameters Sm and Pc have been studied. In addition, statistical tools based on the design of experiments as well as multiple linear regression techniques have been used. Experimental results suggest that the optimal conditions to obtain a minimum Sm of 52.60 gm and a maximum Pc of 190.60 cm(-1) were: 2 A, 5 mu s and 0.4, respectively, for current intensity, pulse time and duty cycle.

Description

Keywords

Roughness, EDM, TiB2, Manufacturing

Department

Ingeniería Mecánica, Energética y de Materiales / Mekanika, Energetika eta Materialen Ingeniaritza

Faculty/School

Degree

Doctorate program

item.page.cita

item.page.rights

© 2017 The Authors. Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license.

Los documentos de Academica-e están protegidos por derechos de autor con todos los derechos reservados, a no ser que se indique lo contrario.